Lithium nickel manganese cobalt oxides
Lithium nickel manganese cobalt oxides (abbreviated NMC, Li-NMC, LNMC, or NCM) are mixed metal oxides of lithium, nickel, manganese and cobalt with the general formula LiNixMnyCo1-x-yO2. These materials are commonly used in lithium-ion batteries for mobile devices and electric vehicles, acting as the positively charged cathode.
There is a particular interest in optimizing NMC for electric vehicle applications because of the material's high energy density and operating voltage. Reducing the cobalt content in NMC is also a current target, owing to ethical issues with cobalt mining and the metal's high cost.[1] Furthermore, an increased nickel content provides more capacity within the stable operation window.[2]
Structure
[edit]NMC materials have layered structures similar to the individual metal oxide compound lithium cobalt oxide (LiCoO2).[3] Lithium ions intercalate between the layers upon discharging, remaining between the lattice planes until the battery gets charged, at which point the lithium de-intercalates and moves to the anode.[4]
Points in a solid solution phase diagram between the end members LiCoO2, LiMnO2, and LiNiO2 represent stoichiometric NMC cathodes.[5] Three numbers immediately following the NMC abbreviation indicate the relative stoichiometry of the three defining metals. For example, an NMC molar composition of 33% nickel, 33% manganese, and 33% cobalt would abbreviate to NMC111 (also NMC333 or NCM333) and have a chemical formula of LiNi 0.33Mn0.33Co 0.33O2. A composition of 50% nickel, 30% manganese, and 20% cobalt would be called NMC532 (or NCM523) and have the formula LiNi0.5Mn0.3Co0.2O2. Other common compositions are NMC622 and NMC811.[4] The general lithium content typically remains around 1:1 with the total transition metal content, with commercial NMC samples usually containing less than 5% excess lithium.[6][7]
For NMC111, the ideal oxidation states for charge distribution are Mn4+, Co3+, and Ni2+. Cobalt and nickel oxidize partially to Co4+ and Ni4+ during charging, while Mn4+ remains inactive and maintains structural stability.[8] Modifying the transition metal stoichiometry changes the material's properties, providing a way to adjust cathode performance.[3] Most notably, increasing the nickel content in NMC increases its initial discharge capacity, but lowers its thermal stability and capacity retention. Increasing cobalt content comes at the cost of replacing either higher-energy nickel or chemically stable manganese while also being expensive. Oxygen can generate from the metal oxide at 300 °C when fully discharged, degrading the lattice. Higher nickel content decreases the oxygen generation temperature while also increasing the heat generation during battery operation.[3] Cation mixing, a process in which Li+ substitutes Ni2+ ions in the lattice, increases as nickel concentration increases as well.[9] The similar size of Ni2+ (0.69 Å) and Li+ (0.76 Å) facilitates cation mixing. Displacing nickel from the layered structure can alter the material's bonding characteristics, forming undesirable phases and lowering its capacity.[10][11]
Synthesis
[edit]The crystallinity, particle size distribution, morphology, and composition all affect the performance of NMC materials, and these parameters can be tuned by using different synthesis methods.[4][12] The first report of nickel manganese cobalt oxide used a coprecipitation method,[13] which is still commonly used today.[14] This method involves dissolving the desired amount of metal precursors together and then drying them to remove the solvent. This material is then blended with a lithium source and heated to temperatures up to 900 °C under oxygen in a process called calcination. Hydroxides, oxalic acid, and carbonates are the most common coprecipitation agents.[14]
Sol-gel methods are another common NMC synthesis method. In this method, transition metal precursors are dissolved in a nitrate or acetate solution, then combined with a lithium nitrate or lithium acetate and citric acid solution. This mixture is stirred and heated to about 80 °C under basic conditions until a viscous gel forms. The gel is dried at around 120 °C and calcined twice, once at 450 °C and again at 800-900 °C, to obtain NMC material.[12]
Hydrothermal treatment can be paired with either the coprecipitation or sol-gel routes. It involves heating the coprecipitate or gel precursors in an autoclave. The treated precursors are then filtered off and calcined normally. Hydrothermal treatments before calcination improves the crystallinity of NMC, which increases the material's performance in cells. However, this comes at the cost of longer material processing times.[12]
History
[edit]NMC cathode materials are historically related to John B. Goodenough's 1980s work on lithium cobalt oxide (LiCoO2),[15] and can be represented as an intergrowth between a layered NaFeO2-type oxide and a closely related lithium rich Li2MnO3 oxide whose amount is related to the initial lithium excess. The first report of Li-rich NMCs was by Zhaolin Liu et. al. from the Institute of Materials Research and Engineering in Singapore in 1999.[13] Further reports of the work of Li-rich NCM cathode material(s) were reported ca. 2000–2001 independently by four research teams:
- At Argonne National Laboratory in the USA a group led by Michael M. Thackeray[16][17] reported these lithium-rich cathodes with the intergrowth structure.
- At Pacific Lithium in New Zealand a team led by Brett Amundsen reported a series of Li(LixCryMnz)O2 layered electrochemically active compounds.[18]
- At Dalhousie University in Canada a team led by Jeff Dahn[19] reported a series of layered cathode materials based on a solid solution formulation of Li(LixMyMnz)O2, where metal M is not chromium.
- A group at Osaka City University led by Tsutomu Ohzuku,[20] who also developed lithium nickel cobalt aluminium oxides.
Properties
[edit]The cell voltage of lithium-ion batteries with NMC cathodes is 3.6–3.7 V.[21]
Arumugam Manthiram has reported that the relative positioning of the metals' 3d bands to the oxygen 2p band leads to each metal's role within NMC cathode materials. The manganese 3d band is above the oxygen 2p band, resulting in manganese's high chemical stability. The cobalt and nickel 3d bands overlap the oxygen 2p band, allowing them to charge to their 4+ oxidation states without the oxygen ions losing electron density.[22]
Usage
[edit]Many electric cars use NMC cathode batteries. NMC batteries were installed in the BMW ActiveE in 2011, and in the BMW i8 starting from 2013.[23] Other electric cars with NMC batteries include, as of 2020: Audi e-tron GE, BAIC EU5 R550, BMW i3, BYD Yuan EV535, Chevrolet Bolt, Hyundai Kona Electric, Jaguar I-Pace, Jiangling Motors JMC E200L, NIO ES6, Nissan Leaf S Plus, Renault ZOE, Roewe Ei5, VW e-Golf and VW ID.3.[24] Only a few electric car manufacturers do not use NMC cathodes in their traction batteries. Tesla is a significant exception, as they use nickel cobalt aluminium oxide and lithium iron phosphate batteries for their vehicles. In 2015, Elon Musk reported that the home storage Tesla Powerwall is based on NMC in order to increase the number of charge/discharge cycles over the life of the units.[24]
Mobile electronics such as mobile phones/smartphones, laptops, and pedelecs can also use NMC-based batteries.[25] These applications almost exclusively used lithium cobalt oxide batteries previously.[26] Another application of NMC batteries is battery storage power stations. Two such storage systems were installed in Korea in 2016 with a combined capacity of 15 MWh.[27] In 2017, a 35 MW NMC battery with a capacity of 11 MWh was installed and commissioned in Newman in the Australian state of Western Australia.[28][29]
See also
[edit]References
[edit]- ^ Warner, John T. (2019-01-01), Warner, John T. (ed.), "Chapter 8 - The materials", Lithium-Ion Battery Chemistries, Elsevier, pp. 171–217, doi:10.1016/b978-0-12-814778-8.00008-9, ISBN 978-0-12-814778-8, S2CID 239383589, retrieved 2023-04-02
- ^ Oswald, Stefan; Gasteiger, Hubert A. (2023-03-01). "The Structural Stability Limit of Layered Lithium Transition Metal Oxides Due to Oxygen Release at High State of Charge and Its Dependence on the Nickel Content". Journal of the Electrochemical Society. 170 (3): 030506. Bibcode:2023JElS..170c0506O. doi:10.1149/1945-7111/acbf80. ISSN 0013-4651. S2CID 258406065.
- ^ a b c Manthiram, Arumugam; Knight, James C.; Myung, Seung-Taek; Oh, Seung-Min; Sun, Yang-Kook (2015-10-07). "Nickel-Rich and Lithium-Rich Layered Oxide Cathodes: Progress and Perspectives". Advanced Energy Materials. 6 (1): 1501010. doi:10.1002/aenm.201501010. S2CID 97342610.
- ^ a b c Warner, John T. (2019-01-01), Warner, John T. (ed.), "Chapter 5 - The Cathodes", Lithium-Ion Battery Chemistries, Elsevier, pp. 99–114, doi:10.1016/b978-0-12-814778-8.00005-3, ISBN 978-0-12-814778-8, S2CID 239420965, retrieved 2023-04-02
- ^ Houchins, Gregory; Viswanathan, Venkatasubramanian (2020-01-01). "Towards Ultra Low Cobalt Cathodes: A High Fidelity Computational Phase Search of Layered Li-Ni-Mn-Co Oxides". Journal of the Electrochemical Society. 167 (7): 070506. arXiv:1805.08171. Bibcode:2020JElS..167g0506H. doi:10.1149/2.0062007JES. ISSN 0013-4651. S2CID 201303669.
- ^ Julien, Christian; Mauger, Alain; Zaghib, Karim; Groult, Henri (2016-07-19). "Optimization of Layered Cathode Materials for Lithium-Ion Batteries". Materials. 9 (7): 595. Bibcode:2016Mate....9..595J. doi:10.3390/ma9070595. ISSN 1996-1944. PMC 5456936. PMID 28773717.
- ^ Li, Xuemin; Colclasure, Andrew M.; Finegan, Donal P.; Ren, Dongsheng; Shi, Ying; Feng, Xuning; Cao, Lei; Yang, Yuan; Smith, Kandler (2019-02-20). "Degradation mechanisms of high capacity 18650 cells containing Si-graphite anode and nickel-rich NMC cathode". Electrochimica Acta. 297: 1109–1120. doi:10.1016/j.electacta.2018.11.194. OSTI 1491439. S2CID 104299816.
- ^ Yoon, Won-Sub; Grey, Clare P.; Balasubramanian, Mahalingam; Yang, Xiao-Qing; Fischer, Daniel A.; McBreen, James (2004). "Combined NMR and XAS Study on Local Environments and Electronic Structures of Electrochemically Li-Ion Deintercalated Li[sub 1−x]Co[sub 1/3]Ni[sub 1/3]Mn[sub 1/3]O[sub 2] Electrode System". Electrochemical and Solid-State Letters. 7 (3): A53. doi:10.1149/1.1643592.
- ^ Zhang, Xiaoyu; Jiang, W. J.; Mauger, A.; Qilu; Gendron, F.; Julien, C. M. (2010-03-01). "Minimization of the cation mixing in Li1+x(NMC)1−xO2 as cathode material". Journal of Power Sources. 195 (5): 1292–1301. Bibcode:2010JPS...195.1292Z. doi:10.1016/j.jpowsour.2009.09.029. ISSN 0378-7753.
- ^ Xu, Bo; Fell, Christopher R.; Chi, Miaofang; Meng, Ying Shirley (2011). "Identifying surface structural changes in layered Li-excess nickel manganese oxides in high voltage lithium ion batteries: A joint experimental and theoretical study". Energy & Environmental Science. 4 (6): 2223. doi:10.1039/c1ee01131f. ISSN 1754-5692.
- ^ Zhao, Enyue; Fang, Lincan; Chen, Minmin; Chen, Dongfeng; Huang, Qingzhen; Hu, Zhongbo; Yan, Qing-bo; Wu, Meimei; Xiao, Xiaoling (2017-01-24). "New insight into Li/Ni disorder in layered cathode materials for lithium ion batteries: a joint study of neutron diffraction, electrochemical kinetic analysis and first-principles calculations". Journal of Materials Chemistry A. 5 (4): 1679–1686. doi:10.1039/C6TA08448F. ISSN 2050-7496.
- ^ a b c Malik, Monu; Chan, Ka Ho; Azimi, Gisele (2022-08-01). "Review on the synthesis of LiNixMnyCo1-x-yO2 (NMC) cathodes for lithium-ion batteries". Materials Today Energy. 28: 101066. doi:10.1016/j.mtener.2022.101066. ISSN 2468-6069. S2CID 249483077.
- ^ a b Liu, Zhaolin; Yu, Aishui; Lee, Jim Y (1999-09-01). "Synthesis and characterization of LiNi1−x−yCoxMnyO2 as the cathode materials of secondary lithium batteries". Journal of Power Sources. 81–82: 416–419. Bibcode:1999JPS....81..416L. doi:10.1016/S0378-7753(99)00221-9. ISSN 0378-7753.
- ^ a b Dong, Hongxu; Koenig, Gary M. (2020). "A review on synthesis and engineering of crystal precursors produced via coprecipitation for multicomponent lithium-ion battery cathode materials". CrystEngComm. 22 (9): 1514–1530. doi:10.1039/C9CE00679F. ISSN 1466-8033. S2CID 198357149.
- ^ Mizushima, K.; Jones, P. C.; Wiseman, P. J.; Goodenough, J. B. (1980-06-01). "LixCoO2 (0". Materials Research Bulletin. 15 (6): 783–789. doi:10.1016/0025-5408(80)90012-4. ISSN 0025-5408. S2CID 97799722.
- ^ US6677082B2, Thackeray, Michael M.; Johnson, Christopher S. & Amine, Khalil et al., "Lithium metal oxide electrodes for lithium cells and batteries", issued 2004-01-13
- ^ US6680143B2, Thackeray, Michael M.; Johnson, Christopher S. & Amine, Khalil et al., "Lithium metal oxide electrodes for lithium cells and batteries", issued 2004-01-20
- ^ Ammundsen, B.; Desilvestro, J.; Groutso, T.; Hassel, D.; Metsen, J.B.; Regan, E.; Steiner, R.; Pickering, P.J. (1999-12-01). "Solid State Synthesis and Properties of Doped LiMnO2 Cathode Materials". MRS Online Proceedings Library. 575: 49–589. doi:10.1557/PROC-575-49.
- ^ US6964828B2, Lu, Zhonghua & Dahn, Jeffrey R., "Cathode compositions for lithium-ion batteries", issued 2005-11-15
- ^ Makimura, Yoshinari; Ohzuku, Tsutomu (2003-06-01). "Lithium insertion material of LiNi1/2Mn1/2O2 for advanced lithium-ion batteries". Journal of Power Sources. Selected papers presented at the 11th International Meeting on Lithium Batteries. 119–121: 156–160. Bibcode:2003JPS...119..156M. doi:10.1016/S0378-7753(03)00170-8. ISSN 0378-7753.
- ^ Miller, Peter (2015-01-01). "Automotive Lithium-Ion Batteries". Johnson Matthey Technology Review. 59 (1): 4–13. doi:10.1595/205651315X685445.
- ^ Manthiram, Arumugam (2020-03-25). "A reflection on lithium-ion battery cathode chemistry". Nature Communications. 11 (1): 1550. Bibcode:2020NatCo..11.1550M. doi:10.1038/s41467-020-15355-0. ISSN 2041-1723. PMC 7096394. PMID 32214093. S2CID 256644096.
- ^ Sakti, Apurba; Michalek, Jeremy J.; Fuchs, Erica R. H.; Whitacre, Jay F. (2015-01-01). "A techno-economic analysis and optimization of Li-ion batteries for light-duty passenger vehicle electrification". Journal of Power Sources. 273: 966–980. Bibcode:2015JPS...273..966S. doi:10.1016/j.jpowsour.2014.09.078. ISSN 0378-7753.
- ^ a b Li, Wangda; Erickson, Evan M.; Manthiram, Arumugam (2020-01-13). "High-nickel layered oxide cathodes for lithium-based automotive batteries". Nature Energy. 5 (1): 26–34. Bibcode:2020NatEn...5...26L. doi:10.1038/s41560-019-0513-0. ISSN 2058-7546. S2CID 256706287.
- ^ Jürgen Garche; Klaus Brandt, eds. (2019). Li-battery safety. Amsterdam, Netherlands: Elsevier. ISBN 978-0-444-64008-6. OCLC 1054022372.
- ^ Patoux, Sébastien; Sannier, Lucas; Lignier, Hélène; Reynier, Yvan; Bourbon, Carole; Jouanneau, Séverine; Le Cras, Frédéric; Martinet, Sébastien (2008-05-01). "High voltage nickel manganese spinel oxides for Li-ion batteries". Electrochimica Acta. 53 (12): 4137–4145. doi:10.1016/j.electacta.2007.12.054. ISSN 0013-4686.
- ^ Kokam (March 7, 2016). "Kokam's 56 Megawatt Energy Storage Project Features World's Largest Lithium NMC Energy Storage System for Frequency Regulation". PR Newswire. Retrieved April 2, 2023.
- ^ Giles Parkinson (2019-08-12). "Alinta sees sub 5-year payback for unsubsidised big battery at Newman". RenewEconomy.
- ^ "Energy Storage Solution Provider" (PDF). Archived from the original (PDF) on 2020-02-23. Retrieved 2020-03-01.