English: Distribution of AA2195 marker wire in an extruded 6061 wire. The marker was inserted into the billet at 1/3 of the billet radius prior to extrusion. The amount of shearing is a function of the extrusion rate relative to the die rotation rate: this ratio increases from a-h.
The person who associated a work with this deed has dedicated the work to the public domain by waiving all of their rights to the work worldwide under copyright law, including all related and neighboring rights, to the extent allowed by law. You can copy, modify, distribute and perform the work, even for commercial purposes, all without asking permission.